Types and Solutions of Robot Welding Defects

      The welding deviation may be caused by the wrong part of the robot welding or the welding machine has a problem. At this time, it is necessary to consider whether the TCP (welding machine positioning point) of the welding robot is accurate, and adjust it in various aspects; if such a thing happens frequently Check the zero position of each axis of the robot, and adjust the zero again.

adb56e1ca40e494edf000fb52100348

    Wrong interface may be caused by wrong main parameters of electric welding and wrong welding machine position. The output power of the welding robot can be adjusted appropriately to change the main parameters of electric welding and welding, and the position of the welding machine and the relative position of the welding machine and the steel parts can be adjusted.

       The occurrence of pores may be caused by poor gas maintenance, too thick topcoat of steel parts or insufficient protective gas, which can be solved by carrying out relative adjustment.

       Excessive splashing may be due to incorrect main parameters of electric welding, multi-component gas or too long welding wire. The output power can be adjusted appropriately to change the main parameters of electric welding, adjust the gas preparation instrument to adjust the proportion of mixed gas, and adjust the welding machine. Opposite parts of steel.

Megmeet welder